+91-9930388308
9:00AM to 7:00PM
Hastelloy Alloy C2000 Sheets Plates Coils, which goes to the obstacle of warm security and weldability. Mechanical ventilation is sensible for Hastelloy C2000 Plates and, under unequivocal conditions, for example, an obliged space, is crucial during welding or cutting activities, or both, to obstruct conceivable prologue to dangerous exhaust, gases, or development that may happen. The prescribed beginning temperature for hot trim is 1232 Degree C (2250 Degree F) and the supported culmination temperature for Hastelloy C2000 Coilsis 954 Degree C (1750 Degree F).
Composite C2000 Plates is astonishing among the versatile nickel-chromium-molybdenum materials in having a purposeful copper augmentation. So as to diminish the precipitation of second stage in the gleam affected welding zones of Alloy C2000 Coils, high between relinquish temperature to 93 Degree C is cherished. Nickel C2000 Sheets >has remarkable mechanical properties at high temperatures, critical for a wide degree of flight and high temperature applications.
The mix of Molybdenum and Copper in Nickel C2000 Plates give astonishing breaking down confirmation from diminishing media, while the high Chromium content gives extraordinary oxidizing obstacle. Nickel C2000 Coils exhibit low entrance characteristics, as necessities be agreeable joint access (weld point) and irrelevant land are proposed.
Precisely when specialists are making gear for Hastelloy UNS N06200 Sheets that can withstand the comprehensive sales that produced arranging can put on a machine, it is immense that the aggregate of the individual pieces inside the machine can hold up after some time.
Specifications | : | ASTM B575 / ASME SB575 |
Size | : | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
Thickness | : | 0.1mm to 12 mm Thk |
Form | : | Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) |
Finish | : | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
Hardness | : | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
STANDARD | UNS | WNR. |
Hastelloy C2000 | N06200 | 2.4675 |
Grade | Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | Si |
Hastelloy C2000 | Remainder | 15.0-17.0 | 14.5-16.5 | 4.0-7.0 | 3.0-4.5 | 2.5 max | 1.0 max | .01 max | .35 max | .04 max | .08 max |
Grade | Tensile Strength | Yield Strength | Elongation at break |
Hastelloy C2000 | 690 MPa | 310 MPa | 45% |