+91-9930388308
9:00AM to 7:00PM
Titanium Grade 2 Plates, which has outstanding disintegrating assurance from sea water, and in like way is used in propeller shafts, fixing and various bits of vessels that are appeared to sea water. Titanium Grade 2 Plates Titanium UNS R50400 Plates is used in steel as an alloying section (ferro-titanium) to reduce grain measure and as a deoxidizer, and in treated steel to diminish carbon content. Titanium Grade 2 Plates is to some degree more grounded than Grade 1 at any rate in like manner use safe against everything examined applications.
Titanium Gr 2 AMS 4902 Plates are used in planes, rockets and rockets where quality, low weight and affirmation from high temperatures are beast. Buy Titanium Alloy Grade 2 Plates at reasonable expense from us. Titanium Grade 2 Plates offers dazzling crippling check, basic formability and quality between examinations 1 and 3.
The decision, low weight degree and remarkable stalling restriction trademark for Grade 2 Titanium Plates has affected a wide and widened measurement of helpful applications which demand a lot of strong execution in restorative framework and fix besides as in flight, vehicle, substance plant, control age, oil and gas extraction, sports, and other bona fide endeavors.
With moderate quality and astonishing hindering imperative and formability, Ti Gr 2 Plates watches out for the most totally used sort of titanium. ASTM B265 GR 2 Plates encounters an allotropic change from the hexagonal close-stuffed alpha stage to the body-centered cubic beta stage at a temperature of 882.5 Degree C (1620.5 Degree F).
STANDARD | WERKSTOFF NR. | UNS |
Titanium Grade 2 | 3.7035 | R50400 |
Grade | C | N | O | H | Ti | Fe | |
Titanium Gr 2 | max | 0.10 | 0.03 | 0.25 | 0.015 | bal | 0.30 |
Min.Tensile(KSI) | Tensile KSI Min |
Yield KSI Min/Max |
Tensile Modulus | Poisson’s Ratio |
50 | 40 | 14.9 | 103 GPa | 0.34-0.10 |
Density | 0.163 lbs/in³ , 4.51 g/cm³ |
Mean Coefficient of Thermal Expansion, in/in/°F (mm/m/°C): | 70- 212°F (20- 100°C): 4.78 x 10-6 (8.6) |
Thermal Conductivity: BTU-in/h-ft-°F (W/m-°K): | At 70°F (21°C): 114(16.4) |
Modulus of Elasticity, ksi (MPa) | 15.2 x 10³(105 x 10³) in tension |
Melting Point | 3040°F (1670°C) |